Clariant Renol CPPR02096 Color concentrate of Titanium Oxide

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol CPPR02096 Color concentrate of Titanium Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application to PolypropyleneData provided by Clariant Masterbatches
Physical Properties Metric English Comments
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F