Chosun Refractories TG-68 Monolithic Refractories for Ladle and Tundish

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories TG-68 Monolithic Refractories for Ladle and Tundish.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.003924 GPa

@Temperature 1500 °C,
Time 10800 sec
0.5691 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 9.81 MPa

@Temperature 1500 °C,
Time 10800 sec
1420 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage -0.350 %

@Temperature 1500 °C,
Time 10800 sec
-0.350 %

@Temperature 2730 °F,
Time 3.00 hour
-0.0500 %

@Temperature 110 °C,
Time 86400 sec
-0.0500 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 65 %
65 %
SiO2 27 %
27 %
Descriptive Properties Value Comments
Installation Method Gunnung, Troweling
Main Applications Tundish Coating
Material Required for Estimating (kg/?) 2,000
Water Required for Casting(%) NOZZLE Mixing