Chosun Refractories SP-3000S High-Adhesion Mortar

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SP-3000S High-Adhesion Mortar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Grain Size 75 µm
75 µm
50% <= 0.075 mm
500 µm
500 µm
2% >= 0.50 mm
Mechanical Properties Metric English Comments
Adhesive Bond Strength 7.848 MPa

@Temperature 500 °C,
Time 10800 sec
1138 psi

@Temperature 932 °F,
Time 3.00 hour
8.829 MPa

@Temperature 110 °C,
Time 86400 sec
1281 psi

@Temperature 230 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Chemical Analysis(%) 45=, 2=
Main Applications Sealing
Refractoriness (SK),Al2O3,Fe2O3 34=