Chosun Refractories SBM-1 Blast Furnace Tap-Hole Refractory

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SBM-1 Blast Furnace Tap-Hole Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 1.87 g/cc
0.0676 lb/in³
Porosity 30 %
30 %
Mechanical Properties Metric English Comments
Compressive Strength 14.7 MPa

@Temperature 1350 °C,
Time 10800 sec
2130 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage 0.10 %

@Temperature 1350 °C,
Time 10800 sec
0.10 %

@Temperature 2460 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 11 %
11 %
SiO2 36 %
36 %
Descriptive Properties Value Comments
Chemical Analysis(%),Si3N4 7
Chemical Analysis(%),SiC+C 46
Main Applications Large Blast Furnace