Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.80 g/cc
0.101 lb/in³
Porosity 17 %
17 %
Mechanical Properties Metric English Comments
Compressive Strength 78.5 MPa
11400 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 5.00 µm/m-°C

@Temperature 1000 °C
2.78 µin/in-°F

@Temperature 1830 °F
Shrinkage -0.300 - 0.30 %

@Temperature 1600 °C,
Time 7200 sec
-0.300 - 0.30 %

@Temperature 2910 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 78 %
78 %
Fe2O3 1.0 %
1.0 %
Descriptive Properties Value Comments
Main Application Lime Kiln, Cement Kiln, Various Rotary kiln
Refractories Under Load(2kg/?,T2?) 1,650
Refractoriness (SK) 39
Users viewing this material also viewed the following: