China Tungsten YG8 Cemented Tungsten Carbide for Mining Purposes

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YG8 Cemented Tungsten Carbide for Mining Purposes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For coring crowns, electrical coal drill bits, coal cutting picks, cone drill bits and scraping knife bits, used in geological prospecting coal mining and oil well boring.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 14.5 - 14.9 g/cc
0.524 - 0.538 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 89
89
Flexural Strength 1470 MPa
213000 psi