China Tungsten Kmo53-A Molybdenum Concentrate

Category Metal , Nonferrous Metal , Molybdenum Alloy
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten Kmo53-A Molybdenum Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Component Elements Properties Metric English Comments
Arsenic, As <= 0.010 %
<= 0.010 %
Bismuth, Bi <= 0.050 %
<= 0.050 %
CaO <= 1.5 %
<= 1.5 %
Copper, Cu <= 0.015 %
<= 0.015 %
Lead, Pb <= 0.15 %
<= 0.15 %
Molybdenum, Mo >= 53 %
>= 53 %
Phosphorous, P <= 0.010 %
<= 0.010 %
Potassium, K <= 38.705 %
<= 38.705 %
SiO2 <= 6.5 %
<= 6.5 %
Tin, Sn <= 0.010 %
<= 0.010 %
Descriptive Properties Value Comments
Tungsten Trioxide, WO3 (%), max 0.05