China Tungsten FeMo70Cu1 Ferro Molybdenum

Category Metal , Nonferrous Metal , Molybdenum Alloy
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten FeMo70Cu1 Ferro Molybdenum.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Copper, Cu <= 1.0 %
<= 1.0 %
Iron, Fe 21.75 - 31.75 %
21.75 - 31.75 %
Molybdenum, Mo 65 - 75 %
65 - 75 %
Phosphorous, P <= 0.050 %
<= 0.050 %
Silicon, Si <= 2.0 %
<= 2.0 %
Sulfur, S <= 0.10 %
<= 0.10 %