Material Notes:
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 16.2 g/cc
0.585 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 1100 MPa
160000 psi
Hard
Modulus of Elasticity 101 GPa
14700 ksi
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000133 ohm-cm
0.0000133 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.00067 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.0045 mV