Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

C.O.I.M. FILCO® 300 Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber Sizing

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer C.O.I.M. S.p.A.
Trade Name FILCO®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. FILCO® 300 Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber Sizing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.Applications: Filco 300 is recommended for sizing of glass fiber to be used for reinforcement of unsaturated polyester and epoxy matrix. Its molecular structure is typical for a highly crystalline polymer in which the oxyranic functions are ranged on both terminal parts and lateral ramifications.The most important applicable properties of Filco 300 are as follows: good degree of affinity with epoxy matrixes employed in the production of glass/resin compoundshigh chemical and hydrolytic resistance of compounds themselvesgood degree of compatibility with various sizing compounds, including the aminic organosilanes in a wide pH rangesuitable for partial self-cross-linking during sizing fiber drying maintaining sufficient residual functionality to bind matrix chemically. This cross-linkage occurs above 130°C.Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Solids Content 39 - 41 %
39 - 41 %
Particle Size 0.70 - 0.90 µm
0.70 - 0.90 µm
pH 5.5 - 7.5
5.5 - 7.5
Viscosity 300 - 500 cP
300 - 500 cP
Descriptive Properties Value Comments
Appearance Milky Liquid
Users viewing this material also viewed the following: