CMW® ELKONITE® 2150 Silver Tungsten contact material ASTM B631, Class C, press-sinter-repress

Category Metal , Metal Matrix Composite , Nonferrous Metal , Precious Metal , Silver Alloy , Refractory Metal , Tungsten Alloy
Manufacturer CMW Inc.
Trade Name ELKONITE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONITE® 2150 Silver Tungsten contact material ASTM B631, Class C, press-sinter-repress.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For electrical ContactsInformation provided by CMW Inc.
Physical Properties Metric English Comments
Density 13.2 g/cc
0.477 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 50
50
Flexural Modulus 0.482 GPa
69.9 ksi
Thermal Properties Metric English Comments
Melting Point >= 980 °C
>= 1800 °F
Solidus 980 °C
1800 °F
Liquidus 3410 °C
6170 °F
Component Elements Properties Metric English Comments
Silver, Ag 50 %
50 %
Tungsten, W 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000287 ohm-cm
0.00000287 ohm-cm
(60% IACS)