CIMBAR BARA 200 Barium Sulfate (BaSO4)

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name BARA
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR BARA 200 Barium Sulfate (BaSO4).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BARA 200 is a natural barium sulfate. Cimbar's BARA 200 is designed to meet all the requirements of drilling grade barite. Bara meets or exceeds all API requirements. These properties make BARA 200 barium sulfate the industry standard for quality and performance in oil field applications and a wide range of other end-use applications.Contains a maximum of 250 mg/kg water soluble Alkaline Earth Metals, such as Calcium.Uses:PlasticsFriction Materials Rubber Urethane FoamsAcoustical CompoundsMold Release AgentsDrilling Fluids and other Oil Field applicationsInformation provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 4.20 g/cc
4.20 g/cc
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Particle Size 6.0 µm
6.0 µm
30% less than 6 microns
Particle Mesh Size 200 Mesh
200 Mesh
3.0% retained
pH 8.0
8.0