Material Notes:
Bostik 140 Low Cost EVA Glue StickLow cost. General purpose for most porous substrates used for craft / floral applications.
Physical Properties Metric English Comments
Viscosity 19000 cP

@Temperature 177 °C
19000 cP

@Temperature 350 °F
Typical
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 68.3 °C
155 °F
Minimum Service Temperature, Air -23.3 °C
-10.0 °F
Processing Properties Metric English Comments
Pot Life 0.17 - 0.50 min
0.17 - 0.50 min
Open Time
Descriptive Properties Value Comments
Color Translucent