BVC 1207-75 has been designed specifically for co-extrusion in vinyl window applications where excellent adhesion to rigid vinyl is required. It has excellent light and heat stability as well as an added biocide for microbial resistance.Information Provided by Bayshore Vinyl Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 78

@Time 10.0 sec
72 - 78

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 14.14 MPa
2051 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
100% Modulus 0.00556 GPa
0.806 ksi
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -29.5 °C
-21.1 °F
Impact Brittleness; ASTM D746