Material Notes:
Formula: C2H4O2CAS: 107-31-3Description: Methylformate pure is a colorless liquid, with an ester-like odor. It is miscible with almost all conventional organic solvents. Synonyms: Methyl methanoate, Formic acid, methyl ester, Ameisensauremethylester, Methanoic acid methyl esterApplications: Non-voc intermediate used in the production of Crop Protection Agents and Pharmaceuticals; Also used as a Resin – bound foundry cores and Blowing agentInformation provided by BASF
Physical Properties Metric English Comments
Density 0.968 g/cc
0.0350 lb/in³
Molecular Weight 60.1 g/mol
60.1 g/mol
Thermal Properties Metric English Comments
Melting Point -100 °C
-148 °F
Boiling Point 32.0 °C
89.6 °F
Flash Point -28.0 °C
-18.4 °F
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
DIN 51 777
Descriptive Properties Value Comments
Assay >97%
Composition Methanol
<3.0%
Ignition Temperature 440°C