Material Notes:
Formula: C26H55NCAS: 900169-60-0Description: Ditridecylamine mixture of isomers is a colorless to yellow liquid with an amine-like odor. It is not miscible with water.Synonyms: 2-Imidazoleidinane, N,N’-Ethyleneurea, 2-Imidazolidone, 2-OxoimidazolidinApplications: Chemical intermediate, Floatation agents, Petroleum additives, Corrosion inhibitor, Plasticizers and SurfactantsInformation provided by BASF
Physical Properties Metric English Comments
Density 0.836 g/cc
0.0302 lb/in³
Molecular Weight 381.7 g/mol
381.7 g/mol
Thermal Properties Metric English Comments
Melting Point <= -45.0 °C
<= -49.0 °F
Boiling Point 220 - 240 °C
428 - 464 °F
Flash Point 138 °C
280 °F
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
DIN 51 777
Descriptive Properties Value Comments
Assay >90%
Composition Tridecane
<0.5%
Tridecanol
<3.0%
Tridecylamine
<3.0%
Tritridecylamine
<10.0%
Ignition Temperature 250°C