Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Austin Novel Materials Texalan® 685A Polyester and Polyether based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 685A Polyester and Polyether based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Physical Properties Metric English Comments
Density 1.18 - 1.22 g/cc
0.0426 - 0.0441 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88
82 - 88
ISO 7619
Tensile Strength >= 36.0 MPa
>= 5220 psi
ISO 37
Tensile Stress >= 5.20 MPa

@Strain 100 %
>= 754 psi

@Strain 100 %
ISO 37
>= 10.0 MPa

@Strain 300 %
>= 1450 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 570 %
>= 570 %
ISO 37
Tear Strength >= 60.0 kN/m
>= 342 pli
ISO 34
K Factor (Wear Factor) <= 55
<= 55
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 40 %

@Temperature 70.0 °C
<= 40 %

@Temperature 158 °F
ISO 815