Material Notes:
Prehardened plastic mould steel with high hardnessApplications: Injection moulds and extrusion dies for thermoplastics. Rubber moulds and blow moulds. Stripper plates in blanking application
Mechanical Properties Metric English Comments
Hardness, Brinell 350 - 410
350 - 410
hardness supplied.