Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Glass AFLAS® MZ TFE/P/VdF Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Asahi Glass Company
Trade Name AFLAS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass AFLAS® MZ TFE/P/VdF Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AFLAS® MZ is a terpolymer composed of tetrafluoroethylene, propylene and vinylidene fluoride. AFLAS® MZ offers a good balance of chemical resistance and improved low temperature performance and is categorized in ASTM D 1418-01 as class FKM, type four.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Mooney Viscosity 50

@Temperature 100 °C
50

@Temperature 212 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Tensile Strength at Break 13.7 MPa
1990 psi
ASTM D638
Elongation at Break 210 %
210 %
ASTM D638
Compression Set 32 %

@Temperature 200 °C
32 %

@Temperature 392 °F
70h
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -13.0 °C
8.60 °F
Descriptive Properties Value Comments
Fluorine Content % 60