Material Notes:
UVISTAKE 7206 is a 100% solid, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic components mounted on printed circuit boards. This system provides an excellent combination of flexibility and strength for demanding applications where toughness is required for the management of the thermomechanical stresses. UVISTAKE 7206 will become tack free when exposed to the proper UV light radiation. Good flexibility for reduced stress in the encapsulation of sensitive glass-bodied components; Highly reversion resistant for good physical stability under high heat and humidity environments; Excellent adhesion to plastic/metal components and substrates; No TDI, no toxic solvents, no free acrylic acid for safetyInformation provided by Aptek Laboratories, Inc.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D1475
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ASTM D2240
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
Cured property; ASTM E831-86
Flash Point >= 100 °C
>= 212 °F
TCC
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Cured property; ASTM D257
Dielectric Constant 3.8

@Frequency 1000 Hz
3.8

@Frequency 1000 Hz
Cured property; ASTM D150
Dielectric Strength >= 59.1 kV/mm

@Thickness 0.0762 mm
>= 1500 kV/in

@Thickness 0.00300 in
Cured; ASTM D149
Dissipation Factor 0.040

@Frequency 1000 Hz
0.040

@Frequency 1000 Hz
Cured property; ASTM D150