AorTech Biomaterials Elast-Eon™ E4 Biomedical Polyurethane Pellets

Category Polymer , Thermoplastic , Polyurethane, TP , Silicone Polyurethane, Ether Based
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AorTech Biomaterials Elast-Eon™ E4 Biomedical Polyurethane Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation.
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Tensile Strength at Break 60.0 MPa
8700 psi
Elongation at Break 25 %
25 %