Ametek P430L P/M Stainless Steel, Sintered from 6.6 g/cc Green Density

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer Ametek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ametek P430L P/M Stainless Steel, Sintered from 6.6 g/cc Green Density.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for 45 minutes. Sintered properties below were determined using transverse rupture bars. Compacting pressure 55 tsi. Green strength 1750 psi. Dimensional change from die size -0.5%.Information provided by Ametek Specialty Metal Products.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 450 MPa
65300 psi
Elongation at Break 3.0 %
3.0 %
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 17 %
17 %
Iron, Fe 82 %
82 %
as balance
Manganese, Mn 0.20 %
0.20 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.90 %
0.90 %
Sulfur, S 0.020 %
0.020 %