AlphaGary Garathane™ GT 5080 A Polyurethane based compound

Category Polymer , Thermoplastic , Polyurethane, TP , Vinyl (PVC)
Manufacturer AlphaGary
Trade Name Garathane™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Garathane™ GT 5080 A Polyurethane based compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC/PU Alloy dull finish
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 59 - 65
59 - 65
Tensile Strength 8.96 MPa
1300 psi
Elongation at Break 350 %
350 %
Flex Crack Resistance 50000
50000
Ross Flex