AlphaGary Garaflex™ O 9940 SA Olefinic Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin , Polyolefin, Wire/Cable Grade
Manufacturer AlphaGary
Trade Name Garaflex™ O
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Garaflex™ O 9940 SA Olefinic Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Garaflex™ O is a flame retarded, olefinic thermoplastic elastomer105°C rated flame retardant olefinic TPE for flat ribbon cable and heat tracing cable
Mechanical Properties Metric English Comments
Hardness, Shore D 43 - 51
43 - 51
Tensile Strength 13.8 MPa
2000 psi
Elongation at Break 500 %
500 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -53.0 °C
-63.4 °F
Oxygen Index 30 %
30 %