AlphaGary Evoprene™ CE 6185 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer AlphaGary
Trade Name Evoprene™ CE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Evoprene™ CE 6185 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Evoprene™ CE range has been specially created to offer processors a cost engineered range of easy processing, fast cycling thermoplastic elastomer compounds for general purpose applications. Evoprene™ CE have high friction characteristics, good electrical resistance, and good ozone resistance.Processing: injection molding, compatible for coinjection with polypropylene.