Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Improved Impact Strength, Low Flash, Low Warpage. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Hollow Articles Under Pressure, Pump HousingsProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Flexural Yield Strength 235 MPa
34100 psi
DIN 53 452
Flexural Modulus 12.0 GPa
1740 ksi
DIN 53 457
Izod Impact, Notched 3.68 J/cm
6.89 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Albis North America Internal Test
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F