Material Notes:
Improved creep strength versus pure niobium. Replacement for pure niobium in applications requiring the chemical resistance of niobium and a material with high melting temperature.Information provided by ATI Wah Chang
Physical Properties Metric English Comments
Density 8.58 g/cc
0.310 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 68.98 GPa

@Temperature 23.0 °C
10000 ksi

@Temperature 73.4 °F
Charpy Impact 210 J

@Temperature 23.0 °C
155 ft-lb

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Thermal Conductivity 41.85 W/m-K
290.4 BTU-in/hr-ft²-°F
Melting Point 2400 - 2420 °C
4350 - 4390 °F
Solidus 2400 °C
4350 °F
Liquidus 2420 °C
4390 °F
Optical Properties Metric English Comments
Emissivity (0-1) 0.103

@Temperature 500 °C
0.103

@Temperature 932 °F
Total Hemispherical
0.11

@Temperature 600 °C
0.11

@Temperature 1110 °F
Total Hemispherical
0.117

@Temperature 700 °C
0.117

@Temperature 1290 °F
Total Hemispherical
0.13

@Temperature 800 °C
0.13

@Temperature 1470 °F
Total Hemispherical
0.142

@Temperature 900 °C
0.142

@Temperature 1650 °F
Total Hemispherical
0.154

@Temperature 100 °C
0.154

@Temperature 212 °F
Total Hemispherical
0.167

@Temperature 1100 °C
0.167

@Temperature 2010 °F
Total Hemispherical
0.179

@Temperature 1200 °C
0.179

@Temperature 2190 °F
Total Hemispherical
Users viewing this material also viewed the following: