ATI Allvac® Vasco® M152 Specialty Steel, Heat Treatment: 691°C (1275°F) Anneal

Category Metal , Ferrous Metal , Stainless Steel
Manufacturer ATI Allvac
Trade Name Vasco®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Vasco® M152 Specialty Steel, Heat Treatment: 691°C (1275°F) Anneal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Rings and structural components for land-based turbines.
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 326
326
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 354
354
Estimated from Rockwell C value.
Hardness, Rockwell C 35
35
Hardness, Vickers 341
341
Estimated from Rockwell C value.
Tensile Strength, Ultimate 1104 MPa
160100 psi
Tensile Strength, Yield 966 MPa

@Strain 0.200 %
140000 psi

@Strain 0.200 %
Elongation at Break 20 %
20 %
Reduction of Area 70 %
70 %
Component Elements Properties Metric English Comments
Carbon, C 0.12 %
0.12 %
Chromium, Cr 16.8 %
16.8 %
Iron, Fe 78 %
78 %
as balance
Manganese, Mn 0.70 %
0.70 %
Molybdenum, Mo 1.8 %
1.8 %
Nickel, Ni 2.5 %
2.5 %
Nitrogen, N 0.030 %
0.030 %
Phosphorous, P 0.013 %
0.013 %
Silicon, Si 0.18 %
0.18 %
Sulfur, S 0.013 %
0.013 %
Vanadium, V 0.33 %
0.33 %