ATI Allvac® Nickelvac® 606 Nickel Superalloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® 606 Nickel Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: Weld wire, woven wire mesh belts.Property values are for samples in the metallurgical condition: 2000°F anneal + water quench.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 8.36 g/cc
0.302 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 70
70
Tensile Strength, Ultimate 759 MPa
110000 psi
Tensile Strength, Yield 276 MPa

@Strain 0.200 %
40000 psi

@Strain 0.200 %
Elongation at Break 55 %
55 %
Reduction of Area 90 %
90 %
Component Elements Properties Metric English Comments
Carbon, C 0.040 %
0.040 %
Chromium, Cr 20 %
20 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe <= 3.0 %
<= 3.0 %
Manganese, Mn 3.0 %
3.0 %
Nb + Ta 2.5 %
2.5 %
Nickel, Ni 67 %
67 %
also includes cobalt
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.010 %
0.010 %
Titanium, Ti 0.30 %
0.30 %