ATI Allvac® 38-644 UNS R58640 Titanium Alloy

Category Metal , Nonferrous Metal , Titanium Alloy , Unalloyed/Modified Titanium
Manufacturer ATI Allvac
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® 38-644 UNS R58640 Titanium Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High-strength, metastable beta alloy. Uses: Spring wire, fasteners, torsion bars for aerospace and automotive applications.Property values are for samples in the metallurgical condition: 1600°F anneal + water quench + age.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 4.81 g/cc
0.174 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 32
32
Tensile Strength, Ultimate 1173 MPa
170100 psi
Tensile Strength, Yield 1104 MPa

@Strain 0.200 %
160100 psi

@Strain 0.200 %
Elongation at Break 8.0 %
8.0 %
Reduction of Area 15 %
15 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.30 %
<= 0.30 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.25 %
<= 0.25 %
Palladium, Pd 0.12 - 0.25 %
0.12 - 0.25 %
Titanium, Ti 99 %
99 %
as balance