ATI Allegheny Ludlum AM 355™ High Strength Alloy, UNS S35500

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AM 355™ High Strength Alloy, UNS S35500.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in sheet and strip. For use in high-strength aerospace applications.Information provided by Allegheny Ludlum
Component Elements Properties Metric English Comments
Chromium, Cr 15.5 %
15.5 %
Iron, Fe 76.5 %
76.5 %
as balance
Manganese, Mn 0.95 %
0.95 %
Molybdenum, Mo 2.75 %
2.75 %
Nickel, Ni 4.3 %
4.3 %