Enhanced version of AL-6NX™, containing a greater concentration of the alloying elements which promote corrosion resistance. Information provided by Allegheny Ludlum
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 21.8 %
21.8 %
Copper, Cu 0.20 %
0.20 %
Iron, Fe >= 45.069 %
>= 45.069 %
As Remainder
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 6.7 %
6.7 %
Nickel, Ni 25.3 %
25.3 %
Nitrogen, N 0.24 %
0.24 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.35 %
0.35 %
Sulfur, S <= 0.0010 %
<= 0.0010 %
Descriptive Properties Value Comments
Critical Crevice Corrosion Temperature, °C 45 (ASTM G48, Practice D)
Acified Ferric Chloride solution, Pickled Mill surface
55 (ASTM G48, Practice B)
Acified Ferric Chloride solution, Pickled Mill surface
Critical Pitting Temperature, °C 90 (ASTM G48, Practice C)
Acified Ferric Chloride solution, Pickled Mill surface
Electrochemical Critical Pitting Temperature, °C 90 (ASTM G150)
1M NaCl solution, Ground Surface
Pitting Resistance Equivalent (PREN) 50.0 Minimum