ATI Allegheny Ludlum 420ESR Tool Steel, UNS S42000

Category Metal , Ferrous Metal , Tool Steel
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum 420ESR Tool Steel, UNS S42000.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This stainless steel grade is an air or oil hardening mold steel having superior internal cleanliness combined with good corrosion resistance. Capable of providing excellent polished surface quality.Information provided by Allegheny Ludlum
Component Elements Properties Metric English Comments
Carbon, C 0.35 %
0.35 %
Chromium, Cr 13 %
13 %
Iron, Fe 87 %
87 %
as balance