3M SS100 Smoke and Sound Sealant

Category Other Engineering Material
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M SS100 Smoke and Sound Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Smoke and Sound Sealant SS 100 is an economical, ready to use, gun-grade, elastomeric sealant that drives to form a monolithic flexible seal that helps prevent unwanted noise infiltration and mitigates the spread of smoke and toxic gas during a fire. 3M Smoke and Sound Sealant SS 100 is designed to seal construction joints and through penetration in non-fire-rated wall and floor assemblies, including smoke partitions and acoustic assemblies. In addition, this product acts as a draftstop to prevent unwanted air movement and provides a barrier against dust and other airborne particulates.Information provided by 3M
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 250 g/l
<= 250 g/l
VOC Less H2O and Exempt Solvents
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.20 MPa
174 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 50.0 °C
122 °F
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Processing Properties Metric English Comments
Shelf Life 18.0 Month

@Temperature 20.0 - 32.2 °C
18.0 Month

@Temperature 68.0 - 90.0 °F
Descriptive Properties Value Comments
Appearance White
Light Gray and Black Flecks