Material Notes:
3M™ Outdoor Masking and Stucco Tape 5959 has a high tensile strength backing for pulling through stucco, EIFS and other heavy coatings. Moisture and UV resistant, strong conformable backing. Clean removal from most opaque surfaces for up to 90 days.Information provided by 3M
Physical Properties Metric English Comments
Thickness 305 microns
12.0 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.4 MPa
2960 psi
Elongation at Break 21 %
21 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Adhesive Type Synthetic rubber
Appearance Red