Material Notes:
3M™ Protective UV Tape 3W55X is a black and white co-extruded polyethylene tape for temporary indoor and outdoor protection of many metals, plastics and glass.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.2 MPa
2490 psi
ASTM D3759
Elongation at Break 450 %
450 %
ASTM D3759
Peel Strength 0.05478 kN/m
0.3125 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Acrylic-Based
Appearance White/Black
Users viewing this material also viewed the following: