Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 2209 Paper Masking Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 2209 Paper Masking Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Paper Masking Tape 2209 is an economy crepe paper tape for holding, bundling, sealing, and non-critical masking jobs where a pressure sensitive tape is needed.Information provided by 3M
Physical Properties Metric English Comments
Thickness 114 microns
4.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.7 MPa
4450 psi
ASTM D3756
Elongation at Break 10.5 %
10.5 %
ASTM D3756
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 66.0 °C
151 °F
for 30 mins
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Tan
Users viewing this material also viewed the following: