Electrical Properties Metric English Comments
Comparative Tracking Index 300 V

@Thickness 3.20 mm
300 V

@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6
Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo..
Comparative Tracking Index 300 V

@Temperature 23.0 °C
300 V

@Temperature 73.4 °F
IEC 60112
DuPont Performance Polymers Crastin® SK601 BK851 PBT  (Unverified Data**)
Crastin® SK601 BK851 is a 10% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers