Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 900 ohm-cm @Temperature 135 °C |
900 ohm-cm @Temperature 275 °F |
ASTM D257 |
LG Chemical LUTENE XL2808BK PE Compound Description: LUTENE XL2808BK has an excellent electrical properties and assists in obtaining a minimum shrink back on aluminum conductor, especially solid conductor. LUTENE XL2808BK is specifically .. |