Electrical Properties Metric English Comments
Volume Resistivity 6.80e+14 ohm-cm

@Temperature 20.0 °C
6.80e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257
Solvay Specialty Polymers Cogegum® GFR/320 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..