Electrical Properties Metric English Comments
Volume Resistivity 6.60e+7 ohm-cm

@Temperature 100 °C
6.60e+7 ohm-cm

@Temperature 212 °F
cured 2 hours @ 93°C
Abatron AboCast 8110-8/AboCure 8110-1 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..
Volume Resistivity 6.60e+7 ohm-cm

@Temperature 150 °C
6.60e+7 ohm-cm

@Temperature 302 °F
cured 2 hours @ 93°C
Abatron AboCast 8110-7/AboCure 8110-1 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..