Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 6.30e+6 ohm-cm @Temperature 250 °C |
>= 6.30e+6 ohm-cm @Temperature 482 °F |
|
Schott ROBAX® Glass Ceramic ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s.. |