Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.50e+13 ohm-cm @Temperature 90.0 °C |
5.50e+13 ohm-cm @Temperature 194 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |