Polymer Property : Volume Resistivity = 40000 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 40000 ohm-cm

@Temperature 350 °C
40000 ohm-cm

@Temperature 662 °F
Corning 7070 Lithia Potash Borosilicate Crushed/Powdered Glass
Available in mesh sizes 4 through 325 and can be customized. Devitrifies before reaching a softening point. Used for sealing and other applications.Information provided by Corning Incorporated.