Electrical Properties Metric English Comments
Volume Resistivity 4.00e+9 ohm-cm

@Temperature 250 °C
4.00e+9 ohm-cm

@Temperature 482 °F
Schott Glass 8095 Lead Glass
Lead glass (28% PbO), electrically highly insulating, highly x-ray absorbing General electrotechnical applicationInformation provided by SCHOTT AG.