Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.00e+14 ohm-cm @Temperature 20.0 °C |
4.00e+14 ohm-cm @Temperature 68.0 °F |
IEC 60502 |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Volume Resistivity | 4.00e+14 ohm-cm @Temperature 105 °C |
4.00e+14 ohm-cm @Temperature 221 °F |
ASTM D257 |
Lord Adhesives Thermoset™ UR-322 Two Component Urethane Potting Compound Lord UR-322 is a two component, room temperature curing urethane potting compound. The cured elastomer is soft, flexible and has a very low modulus at temperatures down to -80°C. Cured UR-322 als.. |