Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.00e+13 ohm-cm @Temperature 66.0 °C |
4.00e+13 ohm-cm @Temperature 151 °F |
|
Abatron AboCast 7703-21/AboCure 7703-22 (B) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Volume Resistivity | 4.00e+13 ohm-cm @Temperature 60.0 °C |
4.00e+13 ohm-cm @Temperature 140 °F |
JIS-K-6723 |
Denka VINYKON W1025 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |