Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 3e+11 ohm-cm @Temperature 150 °C |
>= 3e+11 ohm-cm @Temperature 302 °F |
|
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun.. |