Electrical Properties Metric English Comments
Volume Resistivity 3.70e+16 ohm-cm

@Temperature 23.0 °C
3.70e+16 ohm-cm

@Temperature 73.4 °F
DAM; IEC 60093
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66  (Unverified Data**)
Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf..