Polymer Property : Volume Resistivity = 3.20e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.20e+16 ohm-cm

@Temperature 20.0 °C
3.20e+16 ohm-cm

@Temperature 68.0 °F
Advanced Ceramics ACL 2087 Lithium Alumino-Silicate
A high strength glass-ceramic suitable for sealing to 17% chrome-iron or Nilo 48Information provided by Advanced Ceramics Limited (ACL)